(three) Over a plate attached to the best with the cylinder or long lasting aspect thereof: sufficient Room should be still left to the plate to deliver for stamping at the very least six retest dates: the plate have to be at least one⁄16 inch thick and needs to be connected by welding or by brazing in a temperature of not less than 1100 °F, all through all edges on the plate.
(2) Validate compliance of cylinder shells with all shell requirements; inspect inside before closing in both of those finishes; verify warmth therapy as right; get all samples for all exams and for Verify analyses; witness all tests; validate threads by gauge; report volumetric ability and minimum amount thickness of wall famous.
(iii) When dimensions of cylinder isn't going to permit securing straight specimens, the specimens might be taken in any place or course and may be straightened or flattened chilly by tension only, not by blows.
After strain tests, a flattening examination have to be done on a person cylinder taken at random out of each and every lots of two hundred or much less by inserting the cylinder among wedge-formed knife edges having a 60 diploma incorporated angle, rounded into a half-inch radius.
(iv) Everlasting volumetric expansion may well not exceed 10 % of the entire volumetric enlargement at take a look at force.
The Place of work on the Federal Sign-up publishes documents on behalf of Federal read more agencies but doesn't have any authority around their courses. We suggest you directly Call the company associated with the content material in concern.
(iv) Long-lasting volumetric enlargement may not exceed ten % of the entire volumetric expansion at exam pressure.
(i) The remaining cylinders while in the great deal need to be tested via the evidence strain, water-jacket, or direct growth exam system as prescribed in CGA C-1. The minimum check stress needs to be managed for the specific timeframe as well as the testing machines have to be calibrated as prescribed in CGA C-one.
(2) The dimensions of any centered opening in a head may well not exceed a person 50 % the skin diameter of the cylinder.
(four) As a security precaution, if the manufacturer elects to make this check before the hydrostatic exam, he need to style and design his equipment so which the force is applied to the smallest space practicable, around the point of closure, and to be able to utilize the smallest feasible volume of air or fuel.
(iii) The minimum amount take a look at strain need to be preserved at least thirty seconds and sufficiently for a longer period to make certain total enlargement. Any interior force utilized immediately after warmth-treatment method and just before the Formal check may well not exceed 90 percent with the examination stress.
Reheat treatment method of rejected cylinders is authorized. Subsequent thereto, cylinders need to go all prescribed checks to get satisfactory. Fix by welding or spinning will not be approved.
Cylinders has to be manufactured using gear and processes adequate to make sure that Just about every cylinder made conforms to the requirements of this subpart. No fissure or other defect is permitted that is likely to weaken the concluded container appreciably. The final surface area complete may well not exceed a roughness of 250 RMS. Specific irregularities including draw marks, scratches, pits, and so on., should be held to your minimum in keeping with great higher pressure force vessel production techniques.
Inspection should be carried out on the inside of every container just before closing and externally on Every completed container after heat remedy.